Suture retention strength of expanded polytetraf luoroethylene (ePTFE) graft

Yoshinari Mine, Hideya Mitsui, Yu Oshima, Yasuharu Noishiki, Mikizo Nakai, Shunji Sano

研究成果査読

23 被引用数 (Scopus)

抄録

Our meticulous investigation of ePTFE graft breakage when a wire placed at the edge of an ePTFE graft was pulled, revealed that, depending on the breakage pattern, a break starts much earlier than the peak suture retention strength, which is the current international indicator for anastomotic-site break strength. Furthermore, the breakage patterns differ based on the thickness of the wire and the fiber direction of the ePTFE graft. Based on these findings, we advocate measuring the peak suture retention strength using 0.10-mm sutures and a standardized wire thickness in order to assess the anas-tomotic retention strength of ePTFE grafts.

本文言語English
ページ(範囲)121-128
ページ数8
ジャーナルActa medica Okayama
64
2
出版ステータスPublished - 4月 2010
外部発表はい

ASJC Scopus subject areas

  • 生化学、遺伝学、分子生物学(全般)

フィンガープリント

「Suture retention strength of expanded polytetraf luoroethylene (ePTFE) graft」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル