Marginal gap of recent light-activated restovative glass ionomer immediately after light activation -Effect setting shrinkage and bond strength-

Masao Irie

Research output: Contribution to journalArticle

Original languageEnglish
Pages (from-to)790-794
Number of pages5
JournalThe Journal of the Japanese Society for Dental Materials and Devices
Volume12
Issue number6
Publication statusPublished - 1993

Cite this

@article{20b6d649224d4f2aa21d2b0df43a10fc,
title = "Marginal gap of recent light-activated restovative glass ionomer immediately after light activation -Effect setting shrinkage and bond strength-",
author = "Masao Irie",
year = "1993",
language = "English",
volume = "12",
pages = "790--794",
journal = "The Journal of the Japanese Society for Dental Materials and Devices",
number = "6",

}

TY - JOUR

T1 - Marginal gap of recent light-activated restovative glass ionomer immediately after light activation -Effect setting shrinkage and bond strength-

AU - Irie, Masao

PY - 1993

Y1 - 1993

M3 - Article

VL - 12

SP - 790

EP - 794

JO - The Journal of the Japanese Society for Dental Materials and Devices

JF - The Journal of the Japanese Society for Dental Materials and Devices

IS - 6

ER -