A tube consisted of chitin/chitosan nanofibers is one of the candidates to support nerve regeneration. However, chitin/chitosan would cause inflammation when implanted in human body. This study indicates that chitosan nanofibers (degree of deacetylation; 78% and 93%) could be modified by alternate soaking in calcium and phosphate solutions, resulting in the improvement of their biocompatibility in terms of both in vitro cell culture experiment and in vivo animal test. Deacetylation of the chitosan nanofibers appeared to have little effect on in vitro and in vivo behaviors after 3 days. However, the alternate soaking process clearly improved in vitro and in vivo responses against the chitosan nanofibers. During the process, the surface morphology of the chitosan nanofiber was not changed, i.e. no hydroxyapatite was deposited due to the limited number of soaking. Thus, the surface chemical and physical states of the modified chitosan nanofiber such as surface charge, surface free-energy, and wettability was found to influence both the cell attachment and inflammation.

Original languageEnglish
Pages (from-to)1269-1272
Number of pages4
JournalMaterials Transactions
Volume50
Issue number6
DOIs
Publication statusPublished - Jun 2009
Externally publishedYes

Fingerprint

soaking
Chitosan
biocompatibility
Biocompatibility
Nanofibers
phosphates
Phosphates
chitin
fibers
Fibers
Chitin
nerves
human body
wettability
regeneration
attachment
animals
calcium
free energy
tubes

Keywords

  • Alternate soaking process
  • Chitosan fiber
  • Electrospinning
  • Inflammation
  • Vascular endothelial cell

ASJC Scopus subject areas

  • Materials Science(all)
  • Condensed Matter Physics
  • Mechanical Engineering
  • Mechanics of Materials

Cite this

Improvement of biocompatibility of chitosan fiber modified by ca-phosphate deposition through an alternate soaking process. / Yoshioka, Tomohiko; Onomoto, Hiroshi; Kashiwazaki, Haruhiko; Inoue, Nobuo; Koyama, Yoshihisa; Takakuda, Kazuo; Tanaka, Junzo.

In: Materials Transactions, Vol. 50, No. 6, 06.2009, p. 1269-1272.

Research output: Contribution to journalArticle

Yoshioka, Tomohiko ; Onomoto, Hiroshi ; Kashiwazaki, Haruhiko ; Inoue, Nobuo ; Koyama, Yoshihisa ; Takakuda, Kazuo ; Tanaka, Junzo. / Improvement of biocompatibility of chitosan fiber modified by ca-phosphate deposition through an alternate soaking process. In: Materials Transactions. 2009 ; Vol. 50, No. 6. pp. 1269-1272.
@article{259f0133ec2d4d3f83d87f0b111db401,
title = "Improvement of biocompatibility of chitosan fiber modified by ca-phosphate deposition through an alternate soaking process",
abstract = "A tube consisted of chitin/chitosan nanofibers is one of the candidates to support nerve regeneration. However, chitin/chitosan would cause inflammation when implanted in human body. This study indicates that chitosan nanofibers (degree of deacetylation; 78{\%} and 93{\%}) could be modified by alternate soaking in calcium and phosphate solutions, resulting in the improvement of their biocompatibility in terms of both in vitro cell culture experiment and in vivo animal test. Deacetylation of the chitosan nanofibers appeared to have little effect on in vitro and in vivo behaviors after 3 days. However, the alternate soaking process clearly improved in vitro and in vivo responses against the chitosan nanofibers. During the process, the surface morphology of the chitosan nanofiber was not changed, i.e. no hydroxyapatite was deposited due to the limited number of soaking. Thus, the surface chemical and physical states of the modified chitosan nanofiber such as surface charge, surface free-energy, and wettability was found to influence both the cell attachment and inflammation.",
keywords = "Alternate soaking process, Chitosan fiber, Electrospinning, Inflammation, Vascular endothelial cell",
author = "Tomohiko Yoshioka and Hiroshi Onomoto and Haruhiko Kashiwazaki and Nobuo Inoue and Yoshihisa Koyama and Kazuo Takakuda and Junzo Tanaka",
year = "2009",
month = "6",
doi = "10.2320/matertrans.ME200826",
language = "English",
volume = "50",
pages = "1269--1272",
journal = "Materials Transactions",
issn = "1345-9678",
publisher = "Japan Institute of Metals (JIM)",
number = "6",

}

TY - JOUR

T1 - Improvement of biocompatibility of chitosan fiber modified by ca-phosphate deposition through an alternate soaking process

AU - Yoshioka, Tomohiko

AU - Onomoto, Hiroshi

AU - Kashiwazaki, Haruhiko

AU - Inoue, Nobuo

AU - Koyama, Yoshihisa

AU - Takakuda, Kazuo

AU - Tanaka, Junzo

PY - 2009/6

Y1 - 2009/6

N2 - A tube consisted of chitin/chitosan nanofibers is one of the candidates to support nerve regeneration. However, chitin/chitosan would cause inflammation when implanted in human body. This study indicates that chitosan nanofibers (degree of deacetylation; 78% and 93%) could be modified by alternate soaking in calcium and phosphate solutions, resulting in the improvement of their biocompatibility in terms of both in vitro cell culture experiment and in vivo animal test. Deacetylation of the chitosan nanofibers appeared to have little effect on in vitro and in vivo behaviors after 3 days. However, the alternate soaking process clearly improved in vitro and in vivo responses against the chitosan nanofibers. During the process, the surface morphology of the chitosan nanofiber was not changed, i.e. no hydroxyapatite was deposited due to the limited number of soaking. Thus, the surface chemical and physical states of the modified chitosan nanofiber such as surface charge, surface free-energy, and wettability was found to influence both the cell attachment and inflammation.

AB - A tube consisted of chitin/chitosan nanofibers is one of the candidates to support nerve regeneration. However, chitin/chitosan would cause inflammation when implanted in human body. This study indicates that chitosan nanofibers (degree of deacetylation; 78% and 93%) could be modified by alternate soaking in calcium and phosphate solutions, resulting in the improvement of their biocompatibility in terms of both in vitro cell culture experiment and in vivo animal test. Deacetylation of the chitosan nanofibers appeared to have little effect on in vitro and in vivo behaviors after 3 days. However, the alternate soaking process clearly improved in vitro and in vivo responses against the chitosan nanofibers. During the process, the surface morphology of the chitosan nanofiber was not changed, i.e. no hydroxyapatite was deposited due to the limited number of soaking. Thus, the surface chemical and physical states of the modified chitosan nanofiber such as surface charge, surface free-energy, and wettability was found to influence both the cell attachment and inflammation.

KW - Alternate soaking process

KW - Chitosan fiber

KW - Electrospinning

KW - Inflammation

KW - Vascular endothelial cell

UR - http://www.scopus.com/inward/record.url?scp=68149142648&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=68149142648&partnerID=8YFLogxK

U2 - 10.2320/matertrans.ME200826

DO - 10.2320/matertrans.ME200826

M3 - Article

VL - 50

SP - 1269

EP - 1272

JO - Materials Transactions

JF - Materials Transactions

SN - 1345-9678

IS - 6

ER -