The formation of the 37 angstrom (high-Tc) phase has been studied for Bi:Pb:Sr:Ca:Cu=0.9:0.2:1:1:1.6. The authors obtained the high-Tc phase crystallizing homogeneously in the Pb-induced modulation mode as reported previously. The solid phases formed after each firing treatment at above 795°C were identified, and the melting points of various combinations of these were measured. As a result, the lowest liquid formation temperature was 825°C for a combination of the 24 angstrom phase and Ca2PbO4. The liquid formation and formation of the Pb-substituted 30 angstrom phase seems to be the initial step in formation of the 37 angstrom phase.

Original languageEnglish
Pages (from-to)743-746
Number of pages4
JournalFuntai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy
Volume37
Issue number5
Publication statusPublished - Jul 1990
Externally publishedYes

Fingerprint

Liquids
Melting point
Modulation
Temperature

ASJC Scopus subject areas

  • Mechanical Engineering
  • Metals and Alloys

Cite this

Ito, H., Ikeda, Y., Hiroi, Z., Takano, M., Bando, Y., Takada, J., ... Oda, K. (1990). Formation process of the high-Tc phase in the Bi-Pb-Sr-Ca-Cu-O system. Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 37(5), 743-746.

Formation process of the high-Tc phase in the Bi-Pb-Sr-Ca-Cu-O system. / Ito, Hiroyuki; Ikeda, Yasunori; Hiroi, Zenji; Takano, Mikio; Bando, Yoshichika; Takada, Jun; Egi, Toshio; Kitaguchi, Hitoshi; Oda, Kiichi.

In: Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, Vol. 37, No. 5, 07.1990, p. 743-746.

Research output: Contribution to journalArticle

Ito, H, Ikeda, Y, Hiroi, Z, Takano, M, Bando, Y, Takada, J, Egi, T, Kitaguchi, H & Oda, K 1990, 'Formation process of the high-Tc phase in the Bi-Pb-Sr-Ca-Cu-O system', Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, vol. 37, no. 5, pp. 743-746.
Ito, Hiroyuki ; Ikeda, Yasunori ; Hiroi, Zenji ; Takano, Mikio ; Bando, Yoshichika ; Takada, Jun ; Egi, Toshio ; Kitaguchi, Hitoshi ; Oda, Kiichi. / Formation process of the high-Tc phase in the Bi-Pb-Sr-Ca-Cu-O system. In: Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy. 1990 ; Vol. 37, No. 5. pp. 743-746.
@article{a0a31fc900454c9691ec55134a6f802b,
title = "Formation process of the high-Tc phase in the Bi-Pb-Sr-Ca-Cu-O system",
abstract = "The formation of the 37 angstrom (high-Tc) phase has been studied for Bi:Pb:Sr:Ca:Cu=0.9:0.2:1:1:1.6. The authors obtained the high-Tc phase crystallizing homogeneously in the Pb-induced modulation mode as reported previously. The solid phases formed after each firing treatment at above 795°C were identified, and the melting points of various combinations of these were measured. As a result, the lowest liquid formation temperature was 825°C for a combination of the 24 angstrom phase and Ca2PbO4. The liquid formation and formation of the Pb-substituted 30 angstrom phase seems to be the initial step in formation of the 37 angstrom phase.",
author = "Hiroyuki Ito and Yasunori Ikeda and Zenji Hiroi and Mikio Takano and Yoshichika Bando and Jun Takada and Toshio Egi and Hitoshi Kitaguchi and Kiichi Oda",
year = "1990",
month = "7",
language = "English",
volume = "37",
pages = "743--746",
journal = "Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy",
issn = "0532-8799",
publisher = "Funtai Funamtsu Yakin Kyokai/Japan Soc. of Powder Metallurgy",
number = "5",

}

TY - JOUR

T1 - Formation process of the high-Tc phase in the Bi-Pb-Sr-Ca-Cu-O system

AU - Ito, Hiroyuki

AU - Ikeda, Yasunori

AU - Hiroi, Zenji

AU - Takano, Mikio

AU - Bando, Yoshichika

AU - Takada, Jun

AU - Egi, Toshio

AU - Kitaguchi, Hitoshi

AU - Oda, Kiichi

PY - 1990/7

Y1 - 1990/7

N2 - The formation of the 37 angstrom (high-Tc) phase has been studied for Bi:Pb:Sr:Ca:Cu=0.9:0.2:1:1:1.6. The authors obtained the high-Tc phase crystallizing homogeneously in the Pb-induced modulation mode as reported previously. The solid phases formed after each firing treatment at above 795°C were identified, and the melting points of various combinations of these were measured. As a result, the lowest liquid formation temperature was 825°C for a combination of the 24 angstrom phase and Ca2PbO4. The liquid formation and formation of the Pb-substituted 30 angstrom phase seems to be the initial step in formation of the 37 angstrom phase.

AB - The formation of the 37 angstrom (high-Tc) phase has been studied for Bi:Pb:Sr:Ca:Cu=0.9:0.2:1:1:1.6. The authors obtained the high-Tc phase crystallizing homogeneously in the Pb-induced modulation mode as reported previously. The solid phases formed after each firing treatment at above 795°C were identified, and the melting points of various combinations of these were measured. As a result, the lowest liquid formation temperature was 825°C for a combination of the 24 angstrom phase and Ca2PbO4. The liquid formation and formation of the Pb-substituted 30 angstrom phase seems to be the initial step in formation of the 37 angstrom phase.

UR - http://www.scopus.com/inward/record.url?scp=0025451366&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0025451366&partnerID=8YFLogxK

M3 - Article

AN - SCOPUS:0025451366

VL - 37

SP - 743

EP - 746

JO - Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy

JF - Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy

SN - 0532-8799

IS - 5

ER -