Deformation behavior of multi-layered ceramic capacitors block under non-frame press

Fumio Naruse, Naoya Tada

Research output: Contribution to journalArticle

Abstract

To investigate the deformation behavior of multi-layered ceramic capacitors (MLCCs) during production press process is very important to reduce over all MLCC size and increase the capacity of the MLCC through the enlargement of the electrode area. In the previous paper, the deformation of MLCC blocks in the uniaxial compression test was observed and the filling mechanism was clarified based on the measurement results. In this study, the non-frame press tests of MLCC blocks were carried out to realize the high precision press, in which the lateral compressive stress was given in addition to the longitudinal one. The deformation process was clarified based on the results of cross-sectional observation. In the edge part of the MLCC block, the interlayer space in Side-Gaps L and W was decreased by longitudinal strain and the lateral strain, whereas, at the central part of the MLCC block, the interlayer space in Side-Gaps L and W was decreased only by longitudinal strain. Since the difference in the deformation behavior between the central part and the edge part generated variations in the thickness of MLCC block, the width of the internal electrode part and the width of the Side-Gap, it was concluded that non-frame press was not suitable for high precision press of MLCC block.

Original languageEnglish
Pages (from-to)442-454
Number of pages13
JournalNippon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A
Volume79
Issue number800
DOIs
Publication statusPublished - 2013
Externally publishedYes

Fingerprint

Ceramic capacitors
Electrodes
Compressive stress
Compaction

Keywords

  • Area Fraction
  • Ceramic Dielectric Sheet
  • Deformation Behavior
  • Electrode
  • MLCC
  • Press

ASJC Scopus subject areas

  • Mechanical Engineering
  • Mechanics of Materials
  • Materials Science(all)

Cite this

@article{80ca21ae1b4949e4a0ff08ef578c3773,
title = "Deformation behavior of multi-layered ceramic capacitors block under non-frame press",
abstract = "To investigate the deformation behavior of multi-layered ceramic capacitors (MLCCs) during production press process is very important to reduce over all MLCC size and increase the capacity of the MLCC through the enlargement of the electrode area. In the previous paper, the deformation of MLCC blocks in the uniaxial compression test was observed and the filling mechanism was clarified based on the measurement results. In this study, the non-frame press tests of MLCC blocks were carried out to realize the high precision press, in which the lateral compressive stress was given in addition to the longitudinal one. The deformation process was clarified based on the results of cross-sectional observation. In the edge part of the MLCC block, the interlayer space in Side-Gaps L and W was decreased by longitudinal strain and the lateral strain, whereas, at the central part of the MLCC block, the interlayer space in Side-Gaps L and W was decreased only by longitudinal strain. Since the difference in the deformation behavior between the central part and the edge part generated variations in the thickness of MLCC block, the width of the internal electrode part and the width of the Side-Gap, it was concluded that non-frame press was not suitable for high precision press of MLCC block.",
keywords = "Area Fraction, Ceramic Dielectric Sheet, Deformation Behavior, Electrode, MLCC, Press",
author = "Fumio Naruse and Naoya Tada",
year = "2013",
doi = "10.1299/kikaia.79.442",
language = "English",
volume = "79",
pages = "442--454",
journal = "Nihon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A",
issn = "0387-5008",
publisher = "Japan Society of Mechanical Engineers",
number = "800",

}

TY - JOUR

T1 - Deformation behavior of multi-layered ceramic capacitors block under non-frame press

AU - Naruse, Fumio

AU - Tada, Naoya

PY - 2013

Y1 - 2013

N2 - To investigate the deformation behavior of multi-layered ceramic capacitors (MLCCs) during production press process is very important to reduce over all MLCC size and increase the capacity of the MLCC through the enlargement of the electrode area. In the previous paper, the deformation of MLCC blocks in the uniaxial compression test was observed and the filling mechanism was clarified based on the measurement results. In this study, the non-frame press tests of MLCC blocks were carried out to realize the high precision press, in which the lateral compressive stress was given in addition to the longitudinal one. The deformation process was clarified based on the results of cross-sectional observation. In the edge part of the MLCC block, the interlayer space in Side-Gaps L and W was decreased by longitudinal strain and the lateral strain, whereas, at the central part of the MLCC block, the interlayer space in Side-Gaps L and W was decreased only by longitudinal strain. Since the difference in the deformation behavior between the central part and the edge part generated variations in the thickness of MLCC block, the width of the internal electrode part and the width of the Side-Gap, it was concluded that non-frame press was not suitable for high precision press of MLCC block.

AB - To investigate the deformation behavior of multi-layered ceramic capacitors (MLCCs) during production press process is very important to reduce over all MLCC size and increase the capacity of the MLCC through the enlargement of the electrode area. In the previous paper, the deformation of MLCC blocks in the uniaxial compression test was observed and the filling mechanism was clarified based on the measurement results. In this study, the non-frame press tests of MLCC blocks were carried out to realize the high precision press, in which the lateral compressive stress was given in addition to the longitudinal one. The deformation process was clarified based on the results of cross-sectional observation. In the edge part of the MLCC block, the interlayer space in Side-Gaps L and W was decreased by longitudinal strain and the lateral strain, whereas, at the central part of the MLCC block, the interlayer space in Side-Gaps L and W was decreased only by longitudinal strain. Since the difference in the deformation behavior between the central part and the edge part generated variations in the thickness of MLCC block, the width of the internal electrode part and the width of the Side-Gap, it was concluded that non-frame press was not suitable for high precision press of MLCC block.

KW - Area Fraction

KW - Ceramic Dielectric Sheet

KW - Deformation Behavior

KW - Electrode

KW - MLCC

KW - Press

UR - http://www.scopus.com/inward/record.url?scp=84876920419&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84876920419&partnerID=8YFLogxK

U2 - 10.1299/kikaia.79.442

DO - 10.1299/kikaia.79.442

M3 - Article

AN - SCOPUS:84876920419

VL - 79

SP - 442

EP - 454

JO - Nihon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A

JF - Nihon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A

SN - 0387-5008

IS - 800

ER -