Cutting Mechanism of Sialon with a Single Point Diamond

Toshikatsu Nakajima, Yoshiyuki Uno, Takanori Fujiwara, Atsunori Ikejiri

Research output: Contribution to journalArticle

Abstract

The circular cutting with a single point diamond cutting edge, in which the depth of cut is very small and takes maximum at some point, is carried out for making clear a cutting process of sialon under conditions similar to practical grinding, investigating sliding of a diamond on sialon, chip formation, groove profile, stock removal and so on. Main conclusions obtained in this study are as follows: (1) There are three different regions with depth of cut; elastic, plastic and cutting region. (2) In the transitional cutting process, there are following three types of interference with maximum depth of cut; (i) elastic region through the contact length, (ii) elastic — plastic — elastic, (iii) elastic — plastic — cutting — plastic — elastic. (3) Chips are formed by plastic deformation as well as brittle fracture. (4) Cracks generated under real interference groove become larger with increases of depth of cut and nose radius of cutting edge.

Original languageEnglish
Pages (from-to)1271-1276
Number of pages6
JournalJournal of the Japan Society for Precision Engineering
Volume53
Issue number8
DOIs
Publication statusPublished - Jan 1 1987
Externally publishedYes

Fingerprint

Diamonds
Plastics
Brittle fracture
Plastic deformation
Cracks

Keywords

  • chip
  • circular cutting
  • cutting region
  • elastic region
  • groove profile
  • normally sintered sialon
  • plastic deformation
  • single point diamond
  • transitional cutting process

ASJC Scopus subject areas

  • Mechanical Engineering

Cite this

Cutting Mechanism of Sialon with a Single Point Diamond. / Nakajima, Toshikatsu; Uno, Yoshiyuki; Fujiwara, Takanori; Ikejiri, Atsunori.

In: Journal of the Japan Society for Precision Engineering, Vol. 53, No. 8, 01.01.1987, p. 1271-1276.

Research output: Contribution to journalArticle

Nakajima, Toshikatsu ; Uno, Yoshiyuki ; Fujiwara, Takanori ; Ikejiri, Atsunori. / Cutting Mechanism of Sialon with a Single Point Diamond. In: Journal of the Japan Society for Precision Engineering. 1987 ; Vol. 53, No. 8. pp. 1271-1276.
@article{e0b8f5fc26ac49458cd24e97270ff786,
title = "Cutting Mechanism of Sialon with a Single Point Diamond",
abstract = "The circular cutting with a single point diamond cutting edge, in which the depth of cut is very small and takes maximum at some point, is carried out for making clear a cutting process of sialon under conditions similar to practical grinding, investigating sliding of a diamond on sialon, chip formation, groove profile, stock removal and so on. Main conclusions obtained in this study are as follows: (1) There are three different regions with depth of cut; elastic, plastic and cutting region. (2) In the transitional cutting process, there are following three types of interference with maximum depth of cut; (i) elastic region through the contact length, (ii) elastic — plastic — elastic, (iii) elastic — plastic — cutting — plastic — elastic. (3) Chips are formed by plastic deformation as well as brittle fracture. (4) Cracks generated under real interference groove become larger with increases of depth of cut and nose radius of cutting edge.",
keywords = "chip, circular cutting, cutting region, elastic region, groove profile, normally sintered sialon, plastic deformation, single point diamond, transitional cutting process",
author = "Toshikatsu Nakajima and Yoshiyuki Uno and Takanori Fujiwara and Atsunori Ikejiri",
year = "1987",
month = "1",
day = "1",
doi = "10.2493/jjspe.53.1271",
language = "English",
volume = "53",
pages = "1271--1276",
journal = "Seimitsu Kogaku Kaishi/Journal of the Japan Society for Precision Engineering",
issn = "0912-0289",
publisher = "Japan Society for Precision Engineering",
number = "8",

}

TY - JOUR

T1 - Cutting Mechanism of Sialon with a Single Point Diamond

AU - Nakajima, Toshikatsu

AU - Uno, Yoshiyuki

AU - Fujiwara, Takanori

AU - Ikejiri, Atsunori

PY - 1987/1/1

Y1 - 1987/1/1

N2 - The circular cutting with a single point diamond cutting edge, in which the depth of cut is very small and takes maximum at some point, is carried out for making clear a cutting process of sialon under conditions similar to practical grinding, investigating sliding of a diamond on sialon, chip formation, groove profile, stock removal and so on. Main conclusions obtained in this study are as follows: (1) There are three different regions with depth of cut; elastic, plastic and cutting region. (2) In the transitional cutting process, there are following three types of interference with maximum depth of cut; (i) elastic region through the contact length, (ii) elastic — plastic — elastic, (iii) elastic — plastic — cutting — plastic — elastic. (3) Chips are formed by plastic deformation as well as brittle fracture. (4) Cracks generated under real interference groove become larger with increases of depth of cut and nose radius of cutting edge.

AB - The circular cutting with a single point diamond cutting edge, in which the depth of cut is very small and takes maximum at some point, is carried out for making clear a cutting process of sialon under conditions similar to practical grinding, investigating sliding of a diamond on sialon, chip formation, groove profile, stock removal and so on. Main conclusions obtained in this study are as follows: (1) There are three different regions with depth of cut; elastic, plastic and cutting region. (2) In the transitional cutting process, there are following three types of interference with maximum depth of cut; (i) elastic region through the contact length, (ii) elastic — plastic — elastic, (iii) elastic — plastic — cutting — plastic — elastic. (3) Chips are formed by plastic deformation as well as brittle fracture. (4) Cracks generated under real interference groove become larger with increases of depth of cut and nose radius of cutting edge.

KW - chip

KW - circular cutting

KW - cutting region

KW - elastic region

KW - groove profile

KW - normally sintered sialon

KW - plastic deformation

KW - single point diamond

KW - transitional cutting process

UR - http://www.scopus.com/inward/record.url?scp=85008035987&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=85008035987&partnerID=8YFLogxK

U2 - 10.2493/jjspe.53.1271

DO - 10.2493/jjspe.53.1271

M3 - Article

AN - SCOPUS:85008035987

VL - 53

SP - 1271

EP - 1276

JO - Seimitsu Kogaku Kaishi/Journal of the Japan Society for Precision Engineering

JF - Seimitsu Kogaku Kaishi/Journal of the Japan Society for Precision Engineering

SN - 0912-0289

IS - 8

ER -